Fibreglass wants different water from a concrete pool. Use these ranges from the first fill and through the first weeks, and keep testing after that.
7.2 to 7.4pH
80 to 120Alkalinity ppm
Under 120Calcium ppm
1 to 3Chlorine ppm
| Test | Keep it at | Notes |
|---|---|---|
| pH | 7.2 to 7.4 | The pH control in your equipment package does most of this work. |
| Total alkalinity | 80 to 120 ppm | Holds the pH steady. |
| Calcium hardness | Under 120 ppm | Do not add calcium. Above 120, use a stain and scale control product. The 200 to 400 ppm you will see for concrete pools does not apply to fibreglass. |
| Chlorine | 1 to 3 ppm | Total chlorine. Keep it in range, not above it. |
Start-up
- Have a local pool shop that knows fibreglass do the first clean and water balance, and show you how to look after it.
- Use the test kit in your handover kit, and take a sample to the pool shop whenever the water looks off.
- We talk you through the chlorinator and the filter settings on the phone.
Why it matters
The gelcoat is the smooth interior surface of the shell. Water kept high in pH or chlorine damages it, and damage from chemical imbalance in the water is not covered by the surface warranty. Balanced water keeps the surface, and the warranty, intact. Warranty details.